Precautions for Welding Stainless Steel Pipe

Nov 29, 2023

1. Power supply with vertical external characteristics is adopted, and the positive polarity is adopted for direct current (the welding wire is connected to the negative electrode).

2. Generally suitable for the welding of thin plates below 6mm, with the characteristics of beautiful weld shape and small welding deformation.

3. The shielding gas is argon with a purity of 99.99%. When the welding current is 50~50A, the argon flow rate is 8~0L/min, when the current is 50~250A, the argon flow rate is 2~5L/min.

4. The protruding length of the tungsten electrode from the gas nozzle is preferably 4~5mm. It is 2~3mm for fillet welding and other places with poor shielding performance. It is 5~6mm for deep grooves. The distance from the nozzle to the work is generally not More than 5mm.

5. To prevent the appearance of welding pores. Any rust and oil stains on the welding parts must be cleaned up.

6. For welding arc length, 2~4mm is better when welding ordinary steel, and ~3mm is better when welding stainless steel. If it is too long, the protective effect will not be good.

7. To prevent the backside of the bottom weld bead from being oxidized, the backside needs to be protected by gas.

8. To make the argon gas well protect the welding pool and facilitate the welding operation, the centerline of the tungsten electrode and the welding workpiece should generally maintain an angle of 80~85°, and the angle between the filler wire and the surface of the workpiece should be as small as possible. Generally, it is about 0°.

9. Windproof and ventilation. In windy places, please take measures to block the net, while indoors, you should take appropriate ventilation measures.


For more informations visit:www.threewaysteel.com/www.threeway-steel.com

Nov 29, 2023 -

Seamless Steel Pipes Possess Several Industrial Attributes

Nov 29, 2023 -

The Difference between Hot-dip Plastic Steel Pipe And Plastic-coated Steel Pipe

Nov 29, 2023 -

Causes of Cracking of Stainless Steel Welded Tube

Nov 29, 2023 -

OCTG Casing Running Procedures

Nov 29, 2023 -

Cutting of Large Diameter Seamless Steel Pipe

Nov 22, 2023 -

All About Stainless Hollow Section

Nov 22, 2023 -

Why We Use Seamless Steel Pipe

Nov 22, 2023 -

Seamless Steel Pipes Possess Several Industrial Attributes

Nov 22, 2023 -

The Industrial Characteristics of Carbon Steel Pipes

Nov 22, 2023 -

A106 Vs. A53 -- Welded Vs. Seamless Steel Pipe

2 more news from Threewaysteel »

Apr 29, 2024 -

RAY TECH (MALAYSIA), UNICOMP Technology's first overseas production base officially in operation to follow Belt and Road Initiative

Apr 29, 2024 -

Aven Launches the Cyclops 4K Ultra HD Digital Microscope: Redefining Precision Viewing

Apr 29, 2024 -

SMTA Long Island Chapter Celebrates 30th Anniversary with Membership Appreciation Event

Apr 29, 2024 -

KYZEN Announces Exclusive Partnership with Manufacturers' Representative Restronics Florida

Apr 29, 2024 -

Record Numbers of Exhibitors to Showcase their Products and Services at EWPTE 2024

Apr 29, 2024 -

KYZEN to Promote Pair of Stencil Cleaning Chemistries at SMTA Ciudad Jaurez Expo & Tech Forum

Apr 29, 2024 -

SMTXTRA Partners with Quantum Systems to Expand Representation in Key Territories

Apr 29, 2024 -

SHENMAO Debuts Special Solder Paste for AI Substrate Power Management Modules

Apr 29, 2024 -

IPC Design Competition Champion Crowned at IPC APEX EXPO 2024

Apr 29, 2024 -

Alternative Manufacturing Inc. Awarded QML Requalification to IPC J-STD-001 and IPC-A-610

See electronics manufacturing industry news »

Precautions for Welding Stainless Steel Pipe news release has been viewed 205 times

Global manufacturing solutions provider