We are experiencing fracture problems with 0805 X7R capacito... - Dec 25, 2005 by Mariss
First, when you see the temination on ceramic capacitors cra... - Dec 26, 2005 by davef
That seems to be the case. We are replacing the X7Rs with C0... - Dec 26, 2005 by Mariss
Sure, you can use X7R dielectric ceramic capacitors on mixed... - Dec 26, 2005 by davef
As an alternative theory to the boards being damaged in the ... - Dec 26, 2005 by davef
I'm assuming the fracture in tension; the fracture doesn't s... - Dec 26, 2005 by Mariss
Addendum: The boards are 2" by 2.4" (50mm by 60mm) and ha... - Dec 26, 2005 by Mariss
Putting aside that you want to: * Get this mess cleaned-up ... - Dec 26, 2005 by davef
I would assume you are using a depanelizer to cut the boards... - Dec 27, 2005 by
Agree with Cmiller. We had a similar prob. with some caps. ... - Dec 27, 2005 by
We found the DIP inserter was cracking SMT decoupling caps i... - Dec 28, 2005 by
Your not using a jaw machine? Had a problem with jaw machin... - Dec 28, 2005 by
John brings up a good point. We have seen that problem with ... - Dec 29, 2005 by
Seen cap cracking before. It can be caused by thermal stres... - Dec 30, 2005 by
Hi, Just wondering while reading this thread, would 0402 ... - Jan 02, 2006 by Grant
Yes - as they flex less due to their size. I do have the ca... - Jan 03, 2006 by Rob
Is this a new design or have you manufacted these in the pas... - Jan 03, 2006 by
To recap: 1) The machines use laser centering, not mech j... - Jan 03, 2006 by Mariss
Hi, Id like to see the photos if possible, you can tell a ... - Jan 04, 2006 by
I've seen cracked caps due to de-panelling on caps 40mm in f... - Jan 04, 2006 by
I can't see how prompt washing of the boards could cause a p... - Jan 04, 2006 by Rob
It was suggested that a delay between reflow and washing the... - Jan 04, 2006 by Mariss
To answer your question it was mentioned that allowing the b... - Jan 04, 2006 by RDR
Hi Mariss, "water soluable flux residue to somehow damage... - Jan 05, 2006 by Rob