Hi, I see that the wave angle of the wave solder machine ... - Nov 05, 2005 by Milroy
Typical is 4 to 6 degrees inclination. ... - Nov 05, 2005 by
Hi Ken What exactly the best reffered angle for Sn/Pb & P... - Nov 06, 2005 by Milroy
About the anlge typically is 5-7 depending on the machine. ... - Nov 07, 2005 by LUPO
6 deg is std angle. Some machines have option to adjust angl... - Nov 07, 2005 by PeteC
Milroy, Another thing to look at is your wave profile. Che... - Nov 10, 2005 by
Hi, I`m thinking what would be the best way to avoid icic... - Nov 16, 2005 by Milroy