What is Cu-EFTEC 64T?

Raymond

#28415

What is Cu-EFTEC 64T? | 5 May, 2004

I've been trying to find the metal composition of various lead frames. I keep reading about Cu-EFTEC 64T but can't find any info on it. Does anyone know what material this is?

reply »

#28419

What is Cu-EFTEC 64T? | 5 May, 2004

It's a Furukawa proprietary material. 'Google' on just the 'EFTEC 64T'. [Sometimes it's Cu EFTEC 64T, copper EFTEC 64T, sometimes just EFTEC 64T.] For instance, Table 5-2 in: http://developer.intel.com/design/packtech/ch_05.pdf

reply »

#28450

What is Cu-EFTEC 64T? | 6 May, 2004

Ah, here it is:

EFTEC-64T. A commercial leadframe material with the nominal composition of Cu-0.3Cr-0.25Sn-0.2Zn