hello everybody , i am looking for the elementary caution you need to take when you reflow large board with several thousands of smt components . thank you for your advise

reply »

#3350

Re: large smt board to reflow | 10 August, 2000

Pascal: Two elementary cautines are: 1 Don't dump the board before the reflowed solder is cooled. 2 Try to manage the side to side temperature variations in your oven. I wouldn't be surprised to see 5�C variation.

Good luck

reply »

Reflow Soldering 101 Training Course
High Resolution Fast Speed Industrial Cameras.
High Precision Fluid Dispensers
Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes

Reflow Oven