| Does anybody know a (if possible low-cost) system | which can travel with the PWBs through a reflov oven | (like some temperature profile loggers) for measuring | the residual oxygen? My problem is, it is a batch oven | which does not allow to have any pipes from inside to | an external measuring system. | Thanx, regards | Matthias Mansfeld Matthias: I'm not sure if these suppliers meet your specific requirements, but they make oxygen monitors. They may be able to give you a lead on something that meets your need sbetter. Dave Illinois Instruments 27840 WConcrete Dr Ingleside IL 60041-9907 815.344.6212 fax 6332 Delta F 4 Constitution Way Woburn MA 01801 800.433.2552 fax 781.938.0531