lead free solder

Jacqueline Coia

#14000

lead free solder | 1 October, 1998

Could you tell me please when the lead free solder regulation will become mandatory in Europe and also what are the current industrial alternatives for paste, bar and wire. Cheers, Jack

reply »

CW

#14001

Re: lead free solder | 7 October, 1998

There's a good article on lead-free assembly of mixed technology in the May issue of SMT Magazine (pg. 52)

reply »