Hello, we have increased problems with a product with the p... - Feb 14, 2023 by Yannick Herzog
The slower the squeegee speed the more tendency for "dr... - Feb 14, 2023 by Sr. Tech
the viscosity of the paste is too high, printing parameter i... - Feb 15, 2023 by Wippsen
If these pads are on the edge of the board try increasing th... - Feb 15, 2023 by dima
These guys said most of what I was going to say. I'll add ... - Feb 15, 2023 by ProcEng1
Hello, thank you for your responses. Some time has passed s... - Oct 13, 2023 by Yannick Herzog
Did the paste make it there and did not stick, or the paste ... - Oct 13, 2023 by Evtimov
Is there only 1 pcba affected or more? Can try splitting th... - Oct 16, 2023 by MagyarT
Have you tried making two passes with the blades? ... - Oct 16, 2023 by ProcEng1
Based on these pictures, please check Board/Stencil co-plana... - Oct 16, 2023 by Evtimov
It looks to me that you might have a poorly etched/polished ... - Oct 16, 2023 by AlexV
Just for fun can we see pictures of the blades? ... - Oct 18, 2023 by Stephen
Mass confusion here. Let me drop some knowledge.. #1. Unl... - Oct 19, 2023 by Sr. Tech
I agree, and also, assuming you have SPI (if the solder past... - Oct 20, 2023 by MagyarT
I agree with Sr. Tech. What does the reflowed joint look lik... - Oct 20, 2023 by DWL
Time flies. 25 years ago we would have asked the durometer o... - Oct 23, 2023 by Stephen