Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2320
Can anyone shed any light on the Speed configuration setting... - Oct 25, 2021 by RichC
Here's a link to this section in the manual. https://drive... - Oct 26, 2021 by dontfeedphils
Thanks for the file, it explains pretty much everything we n... - Oct 29, 2021 by RichC
Update - Solved On talking with BTU they mentioned that if ... - Nov 01, 2021 by RichC
Glad to hear it was a cheap and easy fix. ... - Nov 01, 2021 by dontfeedphils
Thanks for posting the solution; this may come in handy some... - Nov 06, 2021 by Tom