Has anyone had much experience of using the "POGO"... - Sep 07, 2021 by leeg
1 ) Component is not Rohs : Material analyzes confirm that t... - Sep 07, 2021 by Djo
Talk to us more about your application. Are you talking abou... - Sep 07, 2021 by davef
Thanks Davef, we are using a mill max pogo pin on a small pc... - Sep 08, 2021 by leeg
So wetting was unstable and slow . You need to do a wettabil... - Sep 08, 2021 by Djo
I did try to attach an image but the option doesn't seem ava... - Sep 08, 2021 by leeg
Use a free cloud service like udrop or wetransfer. From you... - Sep 08, 2021 by kumarb
Strange finish on the pads? So no solder left on the pad? Pa... - Sep 08, 2021 by Stephen
Many pogo pins have a plating that may not solder well. The ... - Sep 08, 2021 by davef
Yes, we soldered some Mil-Max pins on a functional test boar... - Sep 08, 2021 by kyleh04
Slanting Issues after reflow if u are using thru-hole type, ... - Sep 10, 2021 by ylleong
> Slanting Issues after reflow if u are using &am... - Oct 16, 2021 by Jessica
Hi Mr.Bhatia, thanks for your recommend our company! ... - Oct 16, 2021 by Jessica