Optimum solder paste coverage for BGAs | 25 May, 2018

What would be the least and optimum solder paste coverage for good BGA solderability? Are there any studies for that? Thanks.

reply »

#80474

Optimum solder paste coverage for BGAs | 25 May, 2018

1:1 is a good start. A little more info would probably be helpful in answering this query