I'm looking for a No Clean SAC 305 Solder Paste that can be ... - Jan 26, 2018 by Clockwatcher
Sorry to disappoint. No-Clean fluxes are resin-based. They a... - Jan 26, 2018 by Michael
Amtech LF4300 is exactly what your looking for. ... - Jan 26, 2018 by dwl
I still find it weird when people clean "NO clean" - it defe... - Jan 29, 2018 by Evtimov
I believe the correct statement (I've been told) is "the pro... - Jan 30, 2018 by charliem
If you go even further, the flux residue actually isolates t... - Jan 30, 2018 by Evtimov
This is one of the most common questions I get asked. Why cl... - Jan 30, 2018 by Michael
Michael What you say is not a reason for washing. It is a... - Jan 31, 2018 by Stephen
"...electro-chemical migration failures..." Come on Michael... - Jan 31, 2018 by Evtimov
Your right, he is "selling it". Or I should say he is not se... - Feb 01, 2018 by charliem
... >"...electro-chemical migration failures..." Come on Mic... - Feb 01, 2018 by davef
Thank you Davef! That was overreaction to the seller - I don... - Feb 01, 2018 by Evtimov
I've known Mike Konrad for over 20 years. I like him. He is ... - Feb 01, 2018 by davef
Not to be repetitious, I just don't remember if this has bee... - Feb 01, 2018 by davef
Thanks for the kind words Dave. At no point in my reply was ... - Feb 01, 2018 by Michael
Mike, sorry for being aggressive on you! After all we are... - Feb 02, 2018 by Evtimov
Evtimov, no worries. I appreciate your knowledge and contrib... - Feb 02, 2018 by Michael