IS there an IPC standard or equivalent which specifies the m... - Sep 18, 2017 by chintan sanghani
There is no standard minimum / maximum IMC thickness. * T... - Sep 21, 2017 by davef
As far as I know there is no standard thickness minimum or m... - Oct 24, 2017 by Thirdy
You find good information in IPC-4554 that includes recommen... - Dec 05, 2017 by Jan