Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6846
Hi all, We are having a lot of trouble with mis-pick tryi... - Aug 01, 2017 by OrHorti
Are you using a custom nozzle meant for the domed LEDs? If ... - Aug 01, 2017 by dontfeedphils
Can you supply the following information to help with your q... - Aug 01, 2017 by Mark M.
We are using a custom made nozzle, designed for this particu... - Aug 01, 2017 by OrHorti
There is one thing to be checked too. That is to make sure t... - Aug 01, 2017 by Thomas
Agreed with Thomas i increase wait time when picking and slo... - Aug 01, 2017 by Evtimov
A quick and dirty test; Take a few inches of carrier tape... - Aug 01, 2017 by dwl
Try the method I mentioned earlier, it greatly improves most... - Aug 01, 2017 by Thomas
We did this test, we opened the tape and turned it upside ... - Aug 02, 2017 by OrHorti
Are the parts kept in a humidity controlled environment ? P... - Aug 02, 2017 by ProcEng1
I did a test where the leds were put into a 95% humidity at... - Aug 03, 2017 by OrHorti
One tip that I found very useful in this application that ha... - Aug 04, 2017 by tombstonesmt
What was the outcome OrHorti after baking some? ... - Aug 16, 2017 by Mark M.
> What was the outcome OrHorti after baking some? In ... - Sep 01, 2017 by OrHorti
https://youtu.be/aMyoQK_c3hE Did you find the solution? ... - Sep 04, 2017 by Franci Ravnikar
You need to slow down the machine for starters. Try rota... - Sep 06, 2017 by tombstonesmt