Hello experts, Here is my problem: I have a board that ha... - Apr 28, 2017 by Evtimov
Evtimov, The solution you have described is called multiw... - Apr 29, 2017 by Hypnotia
This has already been done. Companies like Seho Selective So... - May 01, 2017 by tombstonesmt
Pavel, that sounds interesting. Do you know anybody worki... - May 01, 2017 by Evtimov
Ectimov, Have you looked into table-top robotic soldering... - May 01, 2017 by SolderingPRO
Hi Evtimov, I've seen lower cost versions around dependin... - May 02, 2017 by Robl
I've always heard this referred to as "stamp soldering". No... - May 02, 2017 by dontfeedphils
Hi Phil, we were given a ball park of approx $125K for a non... - May 03, 2017 by Robl
Evtimov, Check them: ... - May 03, 2017 by Hypnotia
Durastone pallets, we use lots of precision ones for selecti... - May 03, 2017 by Robl
Thank you all! I will ask for quotes and we will see how it ... - May 05, 2017 by Evtimov