Anyone can help me what kind of solder lead use to connect t... - Jan 19, 2015 by Carl
Carl, You can use a high temp solder to connect your T/C'... - Jan 19, 2015 by mac5
Thank you mac. May I know what t/C's your using? Do you h... - Jan 19, 2015 by Carl
Carl, Try this link ... - Jan 20, 2015 by mac5
Kester makes a thermocouple solder: Alloy SN10PB88AG2 Fl... - Jan 21, 2015 by dyoungquist