Hello guys ! I have a problem, I am finding some blow h... - Jan 12, 2011 by Armando_Gomez
How many % were affected? If a few,it can be caused bcoz of... - Jan 12, 2011 by Jacki
We've never seen the defect that you describe, but in wave s... - Jan 13, 2011 by davef
Hi I hope this pictures helps this is the link ... - Jan 20, 2011 by Armando_Gomez
Armando Link does not work. Goes to a "page not found" e... - Jan 20, 2011 by dyoungquist
www.flickr.com/photos/ ... - Jan 21, 2011 by Armando_Gomez
Hi, in my experience, the humidity is trapped in the solder... - Jan 21, 2011 by XPS
Try baking your boards first to remove the moisture. Moistur... - Jan 21, 2011 by aci
Hi In my experience try to change component to another batc... - Jan 23, 2011 by Piter
Hello! I've had the same problem about one Jear ago. We h... - Jan 24, 2011 by Fönsi