I'm just getting into temperature profiling our PCB's. We re... - Dec 10, 2009 by Craig
We like to keep one fully populated SMT golden per product (... - Dec 10, 2009 by SWAG
We use SMD glue to fix our thermocouples to the PCB, pretty ... - Dec 11, 2009 by Loco
I use aluminum tape. Attach the thermocouple to the solder j... - Dec 11, 2009 by Jeff
Thanks for all the replies. I'm wondering how accurate ju... - Dec 11, 2009 by Craig
Here is a link that has a video of the different methods for... - Dec 11, 2009 by KJS123P
I measured the diference soldering the TC to the pad and jus... - Dec 18, 2009 by Fönsi
I would place the TC under the heaviest component if you can... - Dec 18, 2009 by GPost
In a former life, we used hi temp solder. I've heard of adh... - Dec 23, 2009 by Lynn Norman
The negative side to tape is that you could have a small air... - Dec 26, 2009 by Mark
I just read an articale that said using metal tape was bett... - Dec 28, 2009 by WRONGWAY
Why don't you post the link to the article so we can all rea... - Dec 29, 2009 by kpm