I am having some problems with some of my pcbs at ive solder... - Jul 29, 2008 by garyr
Hi, for this kind of issues I will always go with the flu... - Jul 29, 2008 by gabriella
We only use one type of flux for Lead Free. It is an alcoho... - Jul 29, 2008 by garyr
Any other suggestions???? ... - Aug 01, 2008 by garyr
If you are getting top side wetting, I doubt if this is a De... - Aug 04, 2008 by Real Chunks
Patrick, you are right. I am sorry. It is a Water based fl... - Aug 04, 2008 by garyr
Hey Patrick, thanks. The area that is dark (half circle) is... - Aug 04, 2008 by garyr
Have you tried the alcohol based flux on your ive yet? (even... - Aug 05, 2008 by Loco
GR@ICS, can you be mo... - Aug 06, 2008 by Chris1963
We have a 3/6 Nozzle We do have monitors. One of our pots i... - Aug 06, 2008 by garyr
I would have to second the opinion on the water based flux. ... - Aug 08, 2008 by Doug
GR@ICS, I copied a... - Aug 11, 2008 by Chris1963
Too much flux will spatter and can leave balls on either sid... - Aug 11, 2008 by Real Chunks
GR@ICS: Are you dr... - Aug 12, 2008 by Dirk Nuendyke
I would like to thank everyone for their help on this one...... - Aug 20, 2008 by garyr
Let us know what the �sol� was we can all learn from it. ... - Aug 20, 2008 by Patrick Bruneel
use the 2009MLF from Interflux it will take away your solder... - Sep 02, 2008 by Wilma