Is anyone using a laser to selectively solder components to ... - Nov 20, 2007 by dbas
Yes, PROMATION has customer's using laser to solder PCBs. T... - Nov 23, 2007 by Gary
My advice is the technology is not there unless your boards ... - Nov 26, 2007 by James
I agree with James. Granted there are a variety of lasers t... - Nov 26, 2007 by Real Chunks
Well, there seems to be many opinions, many of which could b... - Nov 27, 2007 by Gary
If the goal is selective soldering (not to raise the substra... - Nov 30, 2007 by nas