Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3495
I'm looking for some information on soldering irons being us... - Nov 02, 2006 by robgd3
WE are also going through tips left and right as well with ... - Nov 02, 2006 by RDR
Which solder did you use? What process? Just hand soldering?... - Nov 02, 2006 by
Try Koki S03X7C-56M*** it has colbalt in which prolongs the ... - Nov 03, 2006 by Rob
The process that burnt the tips up yesterday was hand solder... - Nov 03, 2006 by robgd3
The temp your iron is set at is somewhat irrelevant, it is t... - Nov 03, 2006 by RDR
ok, sorry ,750 was deg F and which I said 350~400 were deg C... - Nov 05, 2006 by
*We've tried the WSP80s for leadfree, also SAC. Problem wit... - Nov 06, 2006 by
The key to longer lasting solder tips when using lead free s... - Nov 16, 2006 by