We have these thin and flexible sheets of fiberglass that we... - Oct 02, 2023 by ProcEng1
Hi, I use this Material, you can get a few different types ... - Oct 02, 2023 by Carl_P
We do use that material for fixtures. The stuff I am talkin... - Oct 02, 2023 by ProcEng1
What Is FR4 Substrate Material? FR4, also written as FR-4, i... - Oct 03, 2023 by Assured-Tech
Can you order a blank thin pcb to use as a carrier? ... - Oct 04, 2023 by SMTA-72837649 SMTA
I believe usually board shops will have scrap pieces laying ... - Oct 04, 2023 by Stephen
I ordered some 3mm sheets of Durostone to try. ... - Oct 05, 2023 by ProcEng1
These came in, and they obviously work fine through the oven... - Oct 10, 2023 by ProcEng1
We order bespoke carriers for some of our products, made of ... - Oct 10, 2023 by MagyarT
+1 Durostone ... - Oct 10, 2023 by chicagoindustrial