Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2600
I have noticed on a recent project, the QFN and SOP solder d... - Aug 14, 2023 by calebcSMT
First, this is the result of bad printer setup. Adjust knife... - Aug 14, 2023 by dima
Please elaborate, as I have already tried to rule out printe... - Aug 14, 2023 by calebcSMT
Similar issues arose for me in cases where the contact pads ... - Aug 14, 2023 by dima
the implication being the soldermask is too thick, raising t... - Aug 14, 2023 by calebcSMT
I'm actually currently in the process of discussing with ste... - Aug 14, 2023 by calebcSMT
Now you have to find the root cause, before you continue. Is... - Aug 14, 2023 by Evtimov
I'm curious what you use for PCB Support. Are you using a de... - Aug 23, 2023 by A Very Frazzled Man
Support bars, so essentially the board is sitting ontop of b... - Aug 23, 2023 by calebcSMT
Is there any outcome? ... - Aug 31, 2023 by MagyarT