IHLP wash concerns | 17 February, 2022

Has anyone seen IHLP parts erode like this?

Attachments:

reply »

#87634

IHLP wash concerns | 18 February, 2022

From part documentation: CLEANING INSTRUCTIONS A no clean solder system is recommended for IHLP's. If cleaning must be performed, an Isopropyl alcohol is recommended. If de-ionized Water Wash is used insure it is followed by a thorough warm air dry cycle to avoid oxidation. Some cleaning solutions, especially those containing non-linear alcohol will attack the IHLP and should be avoided. It is recommended that any chemical cleaning solution be thoroughly rinsed with clean water. The IHLP should be tested for compatibility with any cleaning solution before production assembly

reply »

Benchtop Fluid Dispenser
High Throughput Reflow Oven
SMT spare parts - Qinyi Electronics

Conductive Adhesive & Non-Conductive Adhesive Dispensing