Processing Anticapillary or Silicone blocked (SBT) Wire

Views: 857

#83686

Processing Anticapillary or Silicone blocked (SBT) Wire | 5 November, 2019

Does anyone have any experience trying to solder Anticapillary or Silicone Blocked (SBT) wire? It's designed to inhibit wicking of liquids and unfortunately that includes molten solder. We're experimenting with it for a potential high volume application. We need to solder it to a PCB. Or come up with some other wire to PCB interconnect solution. Does anyone want to chime in with any ideas? Thanks!

reply »