Dear Everyone, I'm having problem. the Switch component drop... - Jun 25, 2019 by anhsang38
Do you have any images that show the soldered terminations? ... - Jun 26, 2019 by Steve Thomas
Have some option to fix it by glue with dispenser? Did you c... - Jun 26, 2019 by Panaguru
We are using temperature resistance tape for keeping it. Do ... - Jun 26, 2019 by anhsang38
There are some pictures of solder and pcb terminal after par... - Jun 26, 2019 by anhsang38
Maybe you can change the technological process...first assem... - Jun 27, 2019 by Panaguru
If the case shield is solderable, add pads to the edge of th... - Jun 27, 2019 by SMTA-John SMTA
Thank you Pro, We already think about that, but we can not d... - Jun 27, 2019 by anhsang38
Thank you Pro, Good idea, We will try to do that. ... - Jun 27, 2019 by anhsang38
It seems to me that it would be easier to manually apply a l... - Jun 27, 2019 by Steve Thomas
Wash the board or do what ever to get rid of flux /flux resi... - Jun 27, 2019 by DucHoang
It seems because the soldering area is not enough, so the we... - Aug 23, 2019 by sssamw
We use similar switch and the same oven. You need to modify ... - Sep 06, 2019 by Linux
Hi Do you know in what and where I can find this in IPC stan... - Nov 07, 2019 by Tor