Today I tried to reflow a PCB for the first time. It did not... - Feb 10, 2017 by Deni
I think your problem is that you are using low temperature s... - Feb 10, 2017 by bruce
Perhaps I can add some nitrogen? ... - Feb 10, 2017 by Deni
It looks like you got all the paste to a liquidus stage and ... - Feb 13, 2017 by Evtimov
Den, Just a hunch- I think you might be ramping too fast. ... - Feb 13, 2017 by westshoredesign
That's one way of testing for UL94! ... - Feb 14, 2017 by MikeKeens
Pre-heat, pre-heat, pre-heat! Swap out your acetylene with ... - Feb 14, 2017 by SWAG
I tried several times - it squeaked for a while and then sil... - Feb 15, 2017 by Deni
Get yourself a KIK Oven and Wave Profiler. It will get you ... - Feb 16, 2017 by Murray Northey
Sorry that is spelled KIC not KIK Murray ... - Feb 16, 2017 by Murray Northey
Deni, I would suggest to install bottom heater. The rest ... - Feb 23, 2017 by Hypnotia
Deni, I would suggest N2O over straight Nitrogen, as you ... - Feb 24, 2017 by Robl
Your fixture is pulling too much heat from the assembly. I'd... - Mar 15, 2017 by Steve Thomas
You might want to attempt doing this in a clean room. ... - Apr 28, 2017 by Mark M.