Hello, I am new to this forum, and was hoping to get som... - Nov 23, 2016 by k
Never used stainless pots as when we converted to lead free ... - Nov 27, 2016 by pmcg
We have been using SN100C in our RPS Rhythm selective solder... - Nov 29, 2016 by dyoungquist
Any lead free will eat a leaded designed wave soldering mach... - Nov 30, 2016 by adam
We've run for about 2 years with SN100C on a Stainless pot, ... - Dec 01, 2016 by Robl
Rob Just wondering - have you made analysis of your solde... - Dec 01, 2016 by Stivais
Hi Stivais, Yes, we analyse once a week in 4 pot location... - Dec 01, 2016 by Robl