is it necessary to vacuum seal moisture sensitive components... - Sep 23, 2015 by ehess
Depends on the MSL(Moisture sensitivity level) and how far y... - Sep 23, 2015 by Evtimov
"...air evacuation is not required (Figure 3-5). Light air e... - Sep 23, 2015 by DeanM
Hi, if you seal in proper way, it is not necessarily to vac... - Nov 11, 2015 by Jack.Desiccant