Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2194
I have a 5lb roll of .125" flux core 63/37 solder that I wan... - Jan 18, 2013 by Sr. Tech
I'm not sure, but may be you can exchange it with someone, w... - Jan 18, 2013 by ENIAC
Here's the story: * Solder will melt and alloy with the sol... - Jan 18, 2013 by davef