Hello, does anyone have any information on stress induced du... - Jun 13, 2011 by Travis H
Cracked parts close to the edge on pizza cutters are a commo... - Jun 13, 2011 by KaHrpr
what is the clearance between the chips and the edges? ... - Jun 14, 2011 by Ken
.088" from the edge, running parallel to the V-score, 1812 p... - Jun 14, 2011 by Travis H
Thats .088" from component edge to pcb edge. ... - Jun 14, 2011 by Travis H
I use a pizza cutter with parts closer than that, but they a... - Jun 14, 2011 by isd.jww
Travis H: Are both pads of the component the same distance [... - Jun 14, 2011 by davef
We had a problem with 1825's close to the edge which were be... - Jun 14, 2011 by PRoy
Yes, both pads are the same distance from the edge. I also ... - Jun 15, 2011 by Travis H
This might sound stupid but... We had a similar issue and th... - Jun 15, 2011 by tombstonesmt
Classic mechanical stress crack pattern. Pretty Try bakin... - Jun 15, 2011 by davef
thats very close to the edge. it is preferable to have at le... - Jun 16, 2011 by Ken
One problem you may have with deeper scoring is not so much ... - Jun 17, 2011 by Reese