Hi All Pls advise me about vapor soldering machine if any1 ... - Apr 30, 2010 by Jacki
Fluid suppliers: * 3M||Fluorinert perfluorinate * Dupont|... - Apr 30, 2010 by davef
We are using an Asscon VP800 with Galden LS230 fluid. This ... - Apr 30, 2010 by LarryD
Thanks Larry We are loooking a bigger Vapor machine which c... - May 02, 2010 by Jacki
Does this mean u have to manualy put, the board's coming out... - May 03, 2010 by Sibbe
> Thanks Larry We are loooking a bigger Vapor > mach... - May 03, 2010 by josh
Thanks Josh for your kind advice. Yes, we have some contac... - May 03, 2010 by Jacki
We have a vapor phase machine coming up in auction next week... - May 04, 2010 by X-Line
Thanks the unit from auction is a bit smaller so I'll seek... - May 05, 2010 by Jacki
Why do you want a vapour phase oven? Why not a batch convec... - May 05, 2010 by Stephen
Hi Stephen Our boards are as large as 600x600mm and sometim... - May 05, 2010 by Jacki
Best have a chat to Rehm from their perspective. But galden ... - May 07, 2010 by josh
Hi Josh yes, the cost of galden is a big concern because th... - May 09, 2010 by Jacki