Re: 63/37 paste reflow Is there a standard reccomended ti... - May 09, 2007 by Jim Z
30 to 90 seconds TAL is typical. ... - May 10, 2007 by PeteC
There is no standard for time above liquidus. It is describ... - May 10, 2007 by davef
I have been TAL around 45 to 90 seconds. I prefer the longe... - May 18, 2007 by Ed Faranda
TAL Too Long - dull solder joints, dewetting. TAL Too Short... - May 25, 2007 by mfgengr
Look here: ... - May 28, 2007 by davef