Good afternoon, We run mixed LF/SnPb process for most of ... - Jul 28, 2006 by Hypnotia
What does your reflow profile look like? ... - Jul 28, 2006 by
Two lines of thought are: * That you have some solder conne... - Jul 28, 2006 by davef
Are all these defects related to the trace that enters pad? ... - Jul 28, 2006 by RDR
Good afternoon, Profile is standard ramp-soak-spike (Acco... - Jul 28, 2006 by Hypnotia
Good afternoon, No, defects aren�t trace related. I�ve ju... - Jul 28, 2006 by Hypnotia
Yur profile looks OK for a leaded paste. It may be tyour pa... - Jul 28, 2006 by
Oven is controlled properly. We run a lot of products at thi... - Jul 28, 2006 by Hypnotia
Good afternoon, 1. Yes, most of all I suspect the compone... - Jul 28, 2006 by Hypnotia
Ah, part issue. Good luck, unless you saw these parts being... - Jul 28, 2006 by
No, you can easily find out if it's a part issue - put down ... - Jul 28, 2006 by Rob
Hi Rob, I guess what I meant was if you know it's this re... - Jul 28, 2006 by
Sorry Chunks! Not really with it - Friday afternoon, with... - Jul 28, 2006 by Rob
Yes I agree with the termination problem and the Friday thin... - Jul 28, 2006 by
Please. Why over engineer this the end. Simply wave solder... - Jul 28, 2006 by Dr Shocker
Thats a great idea Doc. If we all listened to your suggesti... - Jul 28, 2006 by
This recipe is nice for leaded soldering. The time above li... - Jul 29, 2006 by davef
Well, a "reflothermal recipe" is a typo. It should read "re... - Jul 29, 2006 by davef
Did you try a different lot of components or a different ven... - Jul 31, 2006 by