I have read some threads about poor wetting on palladium-sil... - May 22, 2006 by
No suggestions, but we've also had problems with silver pall... - May 23, 2006 by
Seems as though the problem is with PCB and not component? ... - May 23, 2006 by RDR
Had exactly the same type of issues. Tried everything from p... - May 23, 2006 by
Sorry I misled you. The PCB pads are wetting, but there is n... - May 23, 2006 by
Not being funny here but I understand exactly what you are s... - May 23, 2006 by
They work well in silver conductive epoxy in hybrid applicat... - May 23, 2006 by Flipit
First, where the temperatures that aare mentioned in the ori... - May 23, 2006 by davef
The temperatures were measured on the board, ~1/2" away from... - May 24, 2006 by
Hi I manufacture ceramic parts that have a terminations tha... - May 25, 2006 by Slaine
The warmest spot you measure on the board is the bare lamina... - May 25, 2006 by davef
Had the same problem with a batch of 0603`s nfrom Vishay. T... - May 25, 2006 by Mark
Print a number of pads of the 0603 on to a ceramic substrate... - May 25, 2006 by Mark
Steve