Electronics Forum: flux residues (Page 74 of 116)

Re: white residue after wash

Electronics Forum | Sun Apr 05 18:59:15 EDT 1998 | Graham Naisbitt

Jaqueline There are so many variables in the electronic assembly manufacturing process involving more than 12 different chemistries, that it is impossible to easily identify and determine the nature and reason of such residues. GEC Hirst Research in

Re: Wave soldering smt components

Electronics Forum | Fri Dec 17 03:38:53 EST 1999 | cklau

Hello Guys; I "ll like to add some comment on Mr John message , see below.. "Be sure that the components to be used on the bottom can take the maximum heat of the wave and the delta T of entering the wave."-John The required preheat temp , that i

Cleaning before Conformal Coating

Electronics Forum | Fri Sep 09 15:50:08 EDT 2005 | chunks

The hand assembled part is soldered in? If so, the white residue may be from the operator using some added wave solder flux to get better wetting when hand soldering.

Re: Residue

Electronics Forum | Tue May 26 16:35:53 EDT 1998 | Ryan Jennens

| | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not localized

wave solder

Electronics Forum | Fri Jun 12 11:15:50 EDT 1998 | Ryan Jennens

Hey all! The wave solder warrior is back. I have found a flux which leave almost no residue (the least yet), but because of its super low solids content I absolutely cannot get topside fillets. The multi-layer, two sided board is on a pallet w

MS2 molten solder surfactant

Electronics Forum | Mon Jan 16 11:00:33 EST 2006 | frankp

Danny, I'm hoping to hear more about this, too. I've seen it mentioned in a couple of other posts, but so far Sara G. (Foresite Inc.) is the only regular SMTNet poster that's actually seen this stuff. Really curious about residues, and what kind of f

Re: Converting to 'No-Clean' process

Electronics Forum | Mon Apr 17 19:46:39 EDT 2000 | Dave F

Murad: Your customer is smart to be concerned about the affect of changing production processes on product reliability. Your Company is smart to inform customers and keep them in the loop about these changes. In developing your demonstration of th

SIR Testing

Electronics Forum | Tue Jul 04 08:04:37 EDT 2006 | davef

The heat from a soldering iron will push raw flux across the surface of the board and into surprising places. It's bad practice to squirt liquid low residue flux on the board during rework, because the portion of the flux that does not get heated pr

how to solder manganin 0.05mm manganin wire to a copper plate

Electronics Forum | Thu Jan 29 09:18:36 EST 2015 | davef

Nichrome, manganin, phosphor bronze etc are easy to solder ... the hard part is removing the corrosion * Manganin: 86% copper, 12% manganese, 2% nickel. Often, it's used in making cryogenic measurements, due to its low heat loss. * Select a flux for

Re: Wave Soldering No-Clean Bottom-Side SMT

Electronics Forum | Tue May 02 12:17:22 EDT 2000 | C.K.

Donnie is correct. "NO-Clean" doesn't translate to "no-residue!"..... who's giving you hassle about this - your ICT guys??!! Residue remaining on your PCB substrate is a function of many different things - flux deposition, solder mask (glossy means


flux residues searches for Companies, Equipment, Machines, Suppliers & Information

High Throughput Reflow Oven

High Resolution Fast Speed Industrial Cameras.
Pillarhouse USA for Selective Soldering Needs

High Throughput Reflow Oven
Best SMT Reflow Oven

World's Best Reflow Oven Customizable for Unique Applications
used smt parts china

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...