looking for HASL TIN thickness specification

Electronics Forum | Wed Sep 03 16:59:13 EDT 2008 | glennster

At a former employer we required HASL thicknes to be a minimum of 0.75 micron (30 microinches), as measured at the thinnest point on any given pad. This would generally assure a minimum 1 year solderability shelf life. Usually when we saw a soldera

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Thu May 28 07:25:58 EDT 1998 | Earl Moon

| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Thu May 28 05:43:33 EDT 1998 | Earl Moon

| Hey yooze guys! | Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) | Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any p

Re: Tin-Lead thickness on PWB's/Let's Hear More

Electronics Forum | Wed May 27 21:05:30 EDT 1998 | Steve Gregory

Hey yooze guys! Enough of the jokes between you and Earl (GRIN), let's get back to the topic...well, okay... you can tell a few more...(but good ones, 'kay?) Anyhoo...I'm not sure if ya'll are on the IPC Technet list or not, I've not seen any posts f

Conformal coating bubbles with 1B73

Electronics Forum | Fri Feb 18 12:00:08 EST 2011 | dennisfo

That has also been the standard here. We have a urethane line which pulls a vacuum on the mixture before transfering to the can. I plan on testing this out before receipt of the 73 thinner. I've also received some feedback with indication that the mi

Conformal coating mask dots and halos

Electronics Forum | Thu Feb 25 10:30:21 EST 2010 | davef

It sounds like your poly dots are secreting something that affects coating thickness. Is this a function of the adhesive used by poly dot supplier?

A concern about conformal coating height

Electronics Forum | Fri Jul 06 10:08:21 EDT 2007 | blnorman

The coating thickness is more a property of the individual coating itself. The 0.03 - 0.13 is based on average properties of acrylics in general. It's like trying to pour 3 mils of motor oil on a table. The material will find it's own thickness.

Bubbles on solder joint(after conformal coating curing)

Electronics Forum | Fri Dec 18 09:07:24 EST 2009 | tommyg_fla

dave, where I work they are having the same problems with 1B31 acrylic. The coating thickness is 6-8 mils dried so that have to do several passes with an air dry between them and a final oven cure. They think that it might be related to the heating r

Bubbles on solder joint(after conformal coating curing)

Electronics Forum | Mon Dec 28 09:12:56 EST 2009 | kpm135

@tommyg_fla According to the TDS the recommended coating thickness for Humiseal 1B31 is only 1-3 mils so if I had to guess I would say your issue might be that you're re-coating over the first pass too soon. All the solvent hasn't evaporated and the

A concern about conformal coating height

Electronics Forum | Thu Jul 05 22:56:53 EDT 2007 | gyverlo

Hello Sirs: Recently we are having an issue with environmental stress (high humidity or moisture), so we decide to apply conformal coating on our motherboard to protect via holes. According to IPC-A-610D, spec of thickness for type AR is 0.03~0.13 m


coating thickness searches for Companies, Equipment, Machines, Suppliers & Information

ISVI High Resolution Fast Speed Industrial Cameras

High Throughput Reflow Oven
PCB Handling Machine with CE

Component Placement 101 Training Course
PCB Handling with CE

World's Best Reflow Oven Customizable for Unique Applications