Full Site - : bga imc (Page 2 of 3)

SAC305 Lead Frame Component with Leaded Process?

Electronics Forum | Tue Sep 16 16:16:12 EDT 2008 | ck_the_flip

Yes, this scenario is fine. However, BGAs are a different story since the ball is the bulk of the solder joint. In this case, you MUST run a "hybrid profile". Look it up in the fine SMTNet archives (keyword: hybrid profile). I have "been there an

Problems with TI DSP modules

Electronics Forum | Wed Oct 24 11:14:44 EDT 2001 | Cemal Basaran

Dave; Thanks for responsding so fast. here are my answers. 1-WOW!!! How do people get these cool toys? I am with the University at Buffalo Electronic Packaging Lab. http://www.packaging.buffalo.edu We have pretty much everything that is sold on the

Over baking BGA- ?

Electronics Forum | Wed Feb 15 09:00:46 EST 2006 | GS

if you look at the J-STD-033B, you will see that such a large PQFP could stay even longer the 24h at 125�C even if internally is already totally dry. It could be, the balls can get oxided and also IMC (Inter metallic compounds) could grow avery littl

Does this forum covers BGA's

Electronics Forum | Mon Feb 21 03:35:38 EST 2005 | abhirami

Thanks Grant and Dave. I have done extensive work on this and found some of the solder balls and solder flux does match my requirements. We have done many tests and have a good responses for both ceramic and plastic substrates. All is fine as long a

PB-Free HASL and Leaded Solder

Electronics Forum | Thu May 13 09:52:34 EDT 2021 | winston_one

Want to update this question a little, I know it appears few years ago, but I hope there is some updates... We have to assembly few samples of motherboards with this kind of finish (customer mistake during pcb order). Normally we can use leaded sold

Question about leaded parts used in leadfree soldering process

Electronics Forum | Thu Apr 20 22:46:26 EDT 2006 | samir

Amol, I thought I answered your question in another thread, dude! Anyway, to re-iterate. Yes, I was able to pull it off a hybrid profile. The LF BGA passed tensile testing, but no, it wasn't thermally cycled or stressed first to expose any latent

Re: Brush-Up Your Intermetalics!!!

Electronics Forum | Thu Jun 17 22:10:48 EDT 1999 | Earl Moon

| | | Does anyone know where I can find a list of things to do to when troubleshooting issues during the wave solder process? | | | | | | for example: | | | | | | Solder Bridge | | | 1.verify amount of flux been aplied. | | | 2.verify turbulance on


bga imc searches for Companies, Equipment, Machines, Suppliers & Information