Electronics Forum: moisture (Page 11 of 135)

Vapor Pressure at lead free reflow temperatures

Electronics Forum | Tue Aug 15 19:07:13 EDT 2006 | vlad_uk

With the added temperature peak associated to Lead free reflow is anyone seeing or concerned about the increased vapor pressure that may result from moisture entrapment in moisture sensitive components?

Tantalum influence on other components

Electronics Forum | Wed Jan 17 05:05:30 EST 2007 | Phil J

The most likely cause is moisture vapor outgassing violently from the Tant package. They are known to be moisture sensitive. Try baking some at 120C overnight and reflowing those.

SMT adhesive suggestions?

Electronics Forum | Fri Jul 20 08:26:52 EDT 2007 | cyber_wolf

SMT adhesive is hydroscopic. Some types absorb moisture faster than others. Moisture+SMT adhesive= pourous adhesive after cure. Excessive cure ramp rates can also contribute to porosity.

problem in solderability

Electronics Forum | Thu Aug 28 13:15:59 EDT 2008 | omid_juve

how can i be sure that the device isn`t affected by moisture ? i mean that if the pins are oxidized due to the moisture how can i remove this oxidization ?

problem in solderability

Electronics Forum | Tue Sep 02 12:43:12 EDT 2008 | stepheniii

That could lead to oxidation of the leads and worsen solderability. It's much better to make sure the components are handled properly and not exposed to moisture. The reason for baking is moisture in the body not in the leads. Why is no one suggest

problem in solderability

Electronics Forum | Wed Sep 03 12:29:47 EDT 2008 | omid_juve

That could lead to oxidation of the leads and > worsen solderability. It's much better to make > sure the components are handled properly and not > exposed to moisture. > > The reason for baking is > moisture in the body not in the leads. > > W

PCB Baking after Wash

Electronics Forum | Thu Dec 04 09:49:11 EST 2008 | lazzara55

Dear Steven: Often the recommendations for baking prior to assembly are derived from various J-stds. But J's currently concern baking moisture out of components, and fail to address the moisture issues of the PCB. Because of that, there is the IPC D

Solder Ball and Splash after Hand Soldering

Electronics Forum | Sat Jul 25 08:47:25 EDT 2009 | davef

Both "moisture content of bare board" and the "thickness of the copper plating in the PTH" are related to each other. As you heat the solder connection, moisture in the board boils and out-gasses through the solder connection. Plating with the proper

smd led storage

Electronics Forum | Thu Mar 18 11:07:45 EDT 2010 | mun4o

hi, lately I have problem with smd leds.After reflow 2-4% of leds are broken.I think , that reason is bad storage of components, because in our stock the tape with leds have not Moisture Barrier Bags.My question is ,how you storage components, which

Silver Immersion Finish - Moisture bake out guideline?

Electronics Forum | Fri Apr 23 17:00:31 EDT 2010 | davef

Hegeman: So you receive these boards in seal moisture barrier bags, store them in a controlled environment, and use them as needed; what is your goal in baking these poor babies?


moisture searches for Companies, Equipment, Machines, Suppliers & Information

High Throughput Reflow Oven

Training online, at your facility, or at one of our worldwide training centers"


High Resolution Fast Speed Industrial Cameras.
Pillarhouse USA for handload Selective Soldering Needs

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
SMT spare parts

Thermal Transfer Materials.