Electronics Forum | Fri Apr 07 16:10:44 EDT 2000 | Chris McDonald
Kapton Tape should not leave a residue. But Ive seem cheap Kapton do that. Anyways I have gotten a stencil cleaner soldevent to clean off tape residue (Multicore has a good one) It will meet IPC. Chris
Electronics Forum | Fri Apr 07 11:52:44 EDT 2000 | Ashok Dhawan
Can anyone suggest a cleaning solvent for removing silicon residue after K Tape has gone through 2 cycles of reflow soldering ? The solvent or cleaning method has to be compliant to IPC Standards - to be used for cleaning gold edge fingers - PCB asse
Industry News | 2013-01-19 07:46:16.0
Information that inspires innovation is center-stage for design, printed boards, electronics assembly, test and printed electronics
Industry News | 2017-02-03 13:13:40.0
Market Leader AdoptSMT will showcase at Southern Manufacturing an array of new innovative products. These products and the service AdoptSMT offers their customers make AdoptSMT’s slogan become true: We keep your production running. AdoptSMT covers the processes of PCB assembly, hand soldering and industrial identification.
Parts & Supplies | Tape and Reel
High Temperature Masking dots High temperature masking tape and dots are ideal for masking gold fingers of printed circuit boards during wave solder or solder dip process, as well as for solder wave masking and electrical insulation. The p
Technical Library | 2013-02-07 17:01:46.0
Silicone contamination is known to have a negative impact on assembly processes such as soldering, adhesive bonding, coating, and wire bonding. In particular, silicone is known to cause de-wetting of materials from surfaces and can result in adhesive failures. There are many sources for silicone contamination with common sources being mold releases or lubricants on manufacturing tools, offgassing during cure of silicone paste adhesives, and residue from pressure sensitive tape. This effort addresses silicone contamination by quantifying adhesive effects under known silicone contaminations. The first step in this effort identified an FT-IR spectroscopic detection limit for surface silicone utilizing the area under the 1263 cm-1 (Si-CH3) absorbance peak as a function of concentration (µg/cm2). The next step was to pre-contaminate surfaces with known concentrations of silicone oil and assess the effects on surface wetting and adhesion. This information will be used to establish guidelines for silicone contamination in different manufacturing areas within Harris Corporation... First published in the 2012 IPC APEX EXPO technical conference proceedings.
Events Calendar | Wed Jun 20 00:00:00 EDT 2018 - Wed Jun 20 00:00:00 EDT 2018 | ,
Consider the options-How should I mask for Conformal Coating?
| https://pcbasupplies.com/jm-20-sn63-pb37-0-4-mm-cored-leaded-solder-wire/
be eliminated Little scattering of solder, very low fume Clear flux residue offers superior cosmetic No Clean Leaded Flux Cored Solder Wire JM-20 Sn63/Pb37 Specs Product name JM-20 Sn63/Pb37 No Clean
ASYMTEK Products | Nordson Electronics Solutions | https://www.nordson.com/en/divisions/adhesive-dispensing-systems/products/melters/minipur-plus-polyurethane-pur-melters
& Woodworking Packaging Bookbinding Paper & Paperboard Converting Tape & Label Stock Textiles Service and Support Aftermarket Solutions Application Testing Adhesive Dispensing Resource Library Legacy Products Literature Search Product Drawings Reconditioned Hot Melt