PTH Voiding Caused by Gold Plated Leads

Electronics Forum | Tue May 21 16:18:57 EDT 2019 | edhare

Interesting problem. I've seen this before on SMT device leads (see Gold Embrittlement paper at http://www.semlab.com). The AuSn4 IMC is solid at typical reflow temperatures and traps volatiles in the solder joint. One usually cannot crank the ref

Problems with TI DSP modules

Electronics Forum | Wed Oct 24 18:08:02 EDT 2001 | davef

1- DF1: WOW!!! How do people get these cool toys? CB: I am with the University at Buffalo Electronic Packaging Lab. http://www.packaging.buffalo.edu We have pretty much everything that is sold on the market as well as Laser inspection technologies we

Problems with TI DSP modules

Electronics Forum | Thu Oct 25 16:48:29 EDT 2001 | Cemal Basaran

We can inspect and measure strain field in anything larger than 320nm with Laser techniques we have. We can do this measurements during fatigue testing. Of course thick intermetallic region as a solid region is a problem due to the fact that you ha

Gold Surface Finish on PCB's

Electronics Forum | Thu Dec 08 07:55:16 EST 2005 | davef

Your understanding of the situation is correct. In both cases, you solder to the nickel. The gold [Au] protects the nickel from oxidation. When soldering, the gold moves into solution in the solder and forms an intermetallic compound [IMC] with th

AuSn solder alloy

Electronics Forum | Tue Dec 30 21:14:22 EST 2003 | davef

You're thinking correctly. 80Au20Sn is incompatible with: * Sn/Pb * In/Sn * Sn/Pb/In * Sn/Pb/Bi Contact your solder supplier to obtain pictures of IMC.

  1  

ausn imc searches for Companies, Equipment, Machines, Suppliers & Information