Electronics Forum | Mon Jun 15 20:37:29 EDT 2020 | travishemen
Try sending your boards to rework before SMT and have them remove the excess solder from the fiducials. It usually works great until someone accidentally removes the entire fiducial.
Electronics Forum | Thu Feb 12 17:21:07 EST 1998 | Justin Medernach
| I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards | before assembly. | + Is it necessary to wash and bake PCB�s before assembly? | + If any, what is the reason for wash and bake of PCB�s? | + If any, wh
Electronics Forum | Tue May 15 11:55:16 EDT 2001 | dason_c
We had a same problem before and Cirtech work with FAB supplier. It is due to the contamination on the tank. No special profile and paste use on the immersion tin board. Dason
Electronics Forum | Mon May 14 17:14:07 EDT 2001 | davef
First, consider checking the fine SMTnet Archives. Look for threads on "white tin", in addition to "immersion tin". We�ve had a cuppla good ones of late. Merix [http://www.merix.com] gives a good comparison of different solderability preservatives
Electronics Forum | Tue Apr 17 10:16:42 EDT 2001 | davef
Welcome to SMTnet. Awww, those assemblers are always whining about something. Just tell him to shut-up and build the blankin� boards. Jeesh!!! We used to have copious archives on the topic on SMTnet and our friend Brian is working his fingers t
Electronics Forum | Mon Apr 26 18:09:07 EDT 2010 | hegemon
Obviously knowledge in this area is still in a bit of a 'flux'. Dave, you had the right idea, the "putz"s signed off on the responsibility, and sent a new batch o'boards. FAST. This new batch were at least date code in 2010, and we had no issues so
Electronics Forum | Fri Apr 23 17:59:54 EDT 2010 | hegemon
Therein lies the issue. Unknown storage conditions before we received the PCBs, date codes just expired (2 weeks), first article is de-lam city! Had a bad feeling about it. Have read some studies showing that there is no linear tie in of visual cha
Electronics Forum | Wed Jul 28 20:56:58 EDT 1999 | Dave F
| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into
Electronics Forum | Thu Jul 29 00:23:45 EDT 1999 | ScottM
| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into
Electronics Forum | Fri Oct 07 08:48:45 EDT 2016 | davef
Two things ... A friend in the contract coating business said: "... the board is not being baked out long enough, 30 min is certainly not long enough depending on how many layers this board is, as the vacuum (from the parylene process) is pulling t
The SMTA membership is a network of professionals who build skills, share practical experience and develop solutions in electronic assembly technologies and related business operations.
Training Provider / Events Organizer / Association / Non-Profit
6600 City W Pkwy
Eden Prairie, MN USA
Phone: 952-920-7682