COB pad contamination from kapton tape adhesive

Electronics Forum | Tue Jul 10 03:51:49 EDT 2007 | vangogh

Hi All, We are producing PCBA with COB process. We are using kapton tape to protect the COB pads from solder splashes/stains. Questions: 1) Is kapton tape an industry accepted way of protecting gold pads from solder splashes? 2) What are the chance

COB pad contamination from kapton tape adhesive

Electronics Forum | Tue Jul 10 07:22:48 EDT 2007 | davef

Q1. Is kapton tape an industry accepted way of protecting gold pads from solder splashes? A1. No. It is more accepted to resolve the reason behind the solder splats, so that the added labor and cost of taping is eliminated. Search the fine SMTnet Arc

kapton dots and liquid solder mask

Electronics Forum | Wed Aug 10 11:57:16 EDT 2005 | pr

Is the peelable mask (put on by the boardhouse) flat on the surface of the pcb? If so can you tell me the material name, so maybe I can find a picture? We have to print adhesive on the board, so the mask has to be flat. That is why Kapton from the b

adhesive for thermocouple

Electronics Forum | Fri Apr 30 18:52:22 EDT 2004 | RicardoF

what about 4 cm of kapton tape on each Thermocouple?

adhesive for thermocouple

Electronics Forum | Fri Apr 30 11:55:55 EDT 2004 | Chris Lampron

Hello Fredrick, I have used several methods of TC attachment including quick set adheasives (not good at reflow temps as Dave suggests) long set two part epoxies (work well if you have the time to wait for a sufficiant cure) temprobes, tape (kapton

No residue low tack adhesive film for registration

Electronics Forum | Thu Feb 15 19:44:50 EST 2001 | davef

I assume Roland [er someone like that] explained on the Main Conference also known as the Forum, the blue "New Thread" button near the middle of the page and 1 1/2" in from the right margin as the preferred way for posting a new thread. [Well, if th

Re: polyimide stencils

Electronics Forum | Sat Nov 14 08:58:38 EST 1998 | Earl Moon

| I keep hearing about polyimide stencils, but what are they like in terms of registration and aperture accuracy? | You are hearing about polyimide as in polyimide film as Kapton (TM Dupont). This material is the stuff of flex and rigid/flex circuit

Re: polyimide stencils

Electronics Forum | Thu Apr 22 15:27:44 EDT 1999 | Hugh M

| | I keep hearing about polyimide stencils, but what are they like in terms of registration and aperture accuracy? | | | You are hearing about polyimide as in polyimide film as Kapton (TM Dupont). This material is the stuff of flex and rigid/flex c

solder on gold finger

Electronics Forum | Fri Apr 13 22:38:19 EDT 2001 | edylc

Hi , Could you be seeing the nickel under the gold plating because you are removing some of the Gold with the Kapton Tape....?? You mean , the adhesive properties of the kapton tape will cause the gold plating on the gold finger to be somehow peel of

Masking with hight temp non silicone tape before wave

Electronics Forum | Wed Feb 18 22:18:26 EST 2009 | davef

"acrylic adhesive" "high temperature" tape

  1 2 3 4 5 6 7 Next

acrylic adhesive kapton searches for Companies, Equipment, Machines, Suppliers & Information

Sell Your Used SMT & Test Equipment

Easily dispense fine pitch components with ±25µm positioning accuracy.
Pillarhouse USA for Selective Soldering Needs

High Throughput Reflow Oven
used smt parts china

World's Best Reflow Oven Customizable for Unique Applications
Voidless Reflow Soldering

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...