Hi Smarts We are having difficulty in reflowing BGA wiht RO... - Jan 07, 2011 by RIPAL
What failure analysis have you done to know that the solder ... - Jan 07, 2011 by ScottE
Consider measuring the temperature of the BGA solder balls d... - Jan 07, 2011 by davef
We havn't done any failure analysis on this BGA. We have thi... - Jan 07, 2011 by RIPAL
we are building only 100 units and there is no scrap board a... - Jan 07, 2011 by RIPAL
Tell your customer that you need five extra assemblies so th... - Jan 07, 2011 by davef
Hi Ripal it seems that you have problem with compatibility ... - Jan 10, 2011 by Piter
Use the Kester solder paste EM828 SAC305. Guarantee good re... - Jan 11, 2011 by Say
Do you think it is because of too much solder. we have 5thou... - Jan 12, 2011 by RIPAL
HI Ok solder past seems to be ok, but what type do you hav... - Jan 12, 2011 by Piter
Hi, We had a similar issue to this. When we examined the boa... - Jan 27, 2011 by richie
good Morning, it looks from the peak temperature that thi... - Feb 01, 2011 by CL