I am reworking some BGAs and just trying to find the easiest... - Jan 13, 2006 by
Flux only works fine. ... - Jan 13, 2006 by RDR
Just tacky flux then? ... - Jan 13, 2006 by
Also is tacky flux the same as gel flux? ... - Jan 13, 2006 by
As far as I have determined, the Gel and Tacky are the same ... - Jan 13, 2006 by RDR
Russ is right. Tacky alone works best. I've done dozens li... - Jan 13, 2006 by URL
Can anyone provide reliability data on this process (flux on... - Jan 13, 2006 by
Hi Ken, Good question, and I did search for what you are... - Jan 14, 2006 by
We are doing a lot of CSP-BGA rework with tacky flux from Se... - Jan 14, 2006 by Mike ZIG
I can't see why it would be any different, You are melting ... - Jan 16, 2006 by RDR
Ken Tacky flux reworked BGA will be perfectly reliable in... - Jan 16, 2006 by davef
Dave, Why does standoff height affect reliability? ... - Jan 16, 2006 by RDR
Dunno. 4% higher standoff results in 16% higher reliability... - Jan 16, 2006 by davef
Thanks for the links! ... - Jan 16, 2006 by RDR
Dave, I would also like to thank you for the links. As ... - Jan 17, 2006 by
What about doing this method on Micro Bgas? ... - Jan 17, 2006 by
Agreed. Some research sugests the "flexibility" of the join... - Jan 17, 2006 by
There are several life studies (see for example ... - Jan 19, 2006 by
Hi James, You can use the same flux for micro BGAs.The 529... - Jan 21, 2006 by Mike ZIG
james