Printed Circuit Board Assembly & PCB Design SMT Electronics Assembly Manufacturing Forum

Printed Circuit Board Assembly & PCB Design Forum

SMT electronics assembly manufacturing forum.


Solderability Test Kit

Chris May

#4600

Solderability Test Kit | 22 March, 2000

Can anyone recommend a solderability test kit.

This would be used for SOT23, chip caps resistors etc;

Thanks in advance,

Chris

reply »

#4601

Re: Solderability Test Kit | 23 March, 2000

Chris: I'm unsure about the kits you seek. Solderability of: * Components: J-STD-002, Dip And Look Method. Malcom Instruments makes a very nice tester. * Boards: IPC TM-650 2.4.12A Solderability, Edge Dip Method

Good luck Dave F

reply »