Hi Guys I am new to SMT Line Currently having a lot of p... - Dec 15, 2005 by aswsteven
What u meant by change every 1.5 day ( Expose to enviroment ... - Dec 15, 2005 by
Hi I mean once I open the jar and load into the print mach... - Dec 15, 2005 by aswsteven
Welcome. A day and a half seems like a very long time to ... - Dec 15, 2005 by davef
A day and half is a life time for our solder paste, Almit V1... - Dec 16, 2005 by snaggletooth
Try to get a sample of Indium and give it a try......i happe... - Dec 16, 2005 by
How about keeping a fridge near the line and only putting on... - Dec 16, 2005 by Rob
Rob The typical warming or stabilization time for solder ... - Dec 16, 2005 by davef
Hi Dave, Sorry, blonde moment. For our prototype line... - Dec 16, 2005 by Rob
Hi Guys My is in line system, printer DEK 265 stencil 4 m... - Dec 17, 2005 by aswsteven