Please give me some guidelines on designing Stencils for Fin... - Dec 08, 2005 by armin
Hi, How fine pitch are you going? What kind of stencil pr... - Dec 08, 2005 by Grant
I'm with Grant on the .005" foil thickness. The key is t... - Dec 08, 2005 by Steve Thomas
Any good stencil house should be able to recommend the prope... - Dec 08, 2005 by Sr. Tech
Start with your board first. Do you have resist/mask betwee... - Dec 08, 2005 by URL
Yes, yes, I agree with American man, URL, on all his points ... - Dec 08, 2005 by
Also the zipper pattern will work too. Samir, why are you... - Dec 08, 2005 by URL
Madam, that's rather forward! By zipper pattern do you me... - Dec 09, 2005 by Rob
Sorry Rob, just what the guys tell me. Yes, on the zipper... - Dec 09, 2005 by URL
I'll rephrase that - you've got rather a lot forward! Tha... - Dec 09, 2005 by Rob
Here are some guidlines: ... - Dec 12, 2005 by PeteC
some of th IPC design guidelines have helped my factory unde... - Dec 14, 2005 by snaggletooth
"find yourself a good stencil manufacturer its there job rea... - Dec 14, 2005 by URL
the original question was: Please give me some guidelines o... - Dec 14, 2005 by snaggletooth
Yup, I saw the original question too. I just can't see how ... - Dec 14, 2005 by URL
Aperatures are often best decided by the stencil manufacture... - Dec 14, 2005 by snaggletooth
Also we have just made a prototype for Wave soldered SMT com... - Dec 14, 2005 by snaggletooth
Snaggletooth, I spent a good portion of my career fightin... - Dec 14, 2005 by
good points but to answer your questions... Although i am a... - Dec 14, 2005 by snaggletooth
Way to go! Now my favorite "deep space nine" website has tur... - Dec 14, 2005 by