We seem to be having a lot of issues with solder not flowing... - Nov 14, 2005 by Mark
What is the finish of the PCB? What type of paste are you u... - Nov 14, 2005 by RDR
Additional questions are: * Does the problem appear with pa... - Nov 14, 2005 by davef