Hi, I`m having some troubles with reflow soldering RQFP-2... - Oct 31, 2005 by Milroy
Shifting? Please describe the "Shifting". I.E. is it cente... - Oct 31, 2005 by URL
If the board is HASL you may always have trouble. Try to re... - Oct 31, 2005 by jdengler
The only problems I've ever had with 208's shifting out of a... - Oct 31, 2005 by Steve Thomas
If I brief shifting, I checked the component before it enter... - Oct 31, 2005 by Milroy
Is an RQFP a Qfp with the center pad for heat dissipation? ... - Nov 01, 2005 by RDR
Is this causing shorts? Or are your pads that wide? ... - Nov 01, 2005 by URL
I just noticed that you mention 2-5mm off, that is huge! It... - Nov 01, 2005 by RDR
What's your pad geometry/sizes relative to lead width/length... - Nov 01, 2005 by moonshine